Browse the Library
Categories > Metal or alloy > Keyword: copper
185 micrographs available, ordered by micrograph number.
Showing 91 - 100 of 185 micrographs | Page 1 .. 7 8 9 10 11 12 13 .. 19 | Previous | Next |
Micrograph
484
:
Cu 80, Sn 20 (wt%) bronze, exhibiting dendritic solidification System: Cu-Sn, Composition: Cu 85, Sn 15 (wt%) Reflected light microscopy 800 μm |
|
Micrograph
485
:
Cu 80, Sn 20 (wt%) bronze, exhibiting dendritic solidification System: Cu-Sn, Composition: Cu 85, Sn 15 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
486
:
Cu 80, Sn 20 (wt%) bronze, exhibiting dendritic solidification System: Cu-Sn, Composition: Cu 85, Sn 15 (wt%) Reflected light microscopy 100 μm |
|
Micrograph
487
:
Cu 85, Sn 15 (wt%) bronze, annealed at 650°C System: Cu-Sn, Composition: Cu 85, Sn 15 (wt%) Reflected light microscopy 800 μm |
|
Micrograph
488
:
Cu 85, Sn 15 (wt%) bronze, annealed at 650°C System: Cu-Sn, Composition: Cu 85, Sn 15 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
489
:
Cu 85, Sn 15 (wt%) bronze, annealed at 650°C System: Cu-Sn, Composition: Cu 85, Sn 15 (wt%) Reflected light microscopy 100 μm |
|
Micrograph
490
:
Cu 85, Sn 15 (wt%) bronze, annealed System: Cu-Sn, Composition: Cu 85, Sn 15 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
491
:
Cu 70, Sn 30 (wt%) bronze, as cast System: Cu-Sn, Composition: Cu 70, Sn 30 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
492
:
Cu 70, Sn 30 (wt%) bronze, as cast System: Cu-Sn, Composition: Cu 70, Sn 30 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
493
:
Cu 70, Sn 30 (wt%) bronze, as cast System: Cu-Sn, Composition: Cu 70, Sn 30 (wt%) Reflected light microscopy 100 μm |
Showing 91 - 100 of 185 micrographs | Page 1 .. 7 8 9 10 11 12 13 .. 19 | Previous | Next |
Help is available on browsing.
Alternatively, search the Library (from top right on any page), or use advanced search.