Browse the Library
Categories > Metal or alloy > Keyword: aluminium
60 micrographs available, ordered by micrograph number.
Showing 51 - 60 of 60 micrographs | Page 1 2 3 4 5 6 | Previous | Next |
Micrograph
668
:
Al-90 wt% Cu (bronze) System: Al-Cu, Composition: Al 10, Cu 90 (wt%) Reflected light microscopy 50 μm |
|
Micrograph
669
:
Al-90 wt% Cu (bronze) System: Al-Cu, Composition: Al 10, Cu 90 (wt%) Reflected light microscopy 20 μm |
|
Micrograph
710
:
Wrought-grade aluminium alloy (Al-Mg-Fe-Si containing < 1wt.% of each solute); refined with TiB2 particles. Deformation of grain structure is due to cutting of sample with scissors. System: Al-Mg-Fe-Si, Composition: Not specified Cross-polarised light microscopy 400 μm |
|
Micrograph
711
:
As-cast wrought-grade aluminium alloy (Al-Mg-Fe-Si containing < 1wt.% of each solute). No addition of grain refinement particles (e.g. TiB2). System: Al-Mg-Fe-Si, Composition: Not specified Cross-polarised light microscopy 1 mm |
|
Micrograph
712
:
As-cast wrought-grade aluminium alloy (Al-Mg-Fe-Si containing < 1wt.% of each solute). Addition of TiB2 particles facilitates the formation of a fine, equiaxed grain structure (grain refinement). System: Al-Mg-Fe-Si, Composition: Not specified Cross-polarised light microscopy 400 μm |
|
Micrograph
841
:
Micrograph of base material microstructure: H32 - cold-worked and stabilised to obtain 1/4 hardness. System: Al-Mg, Composition: Al, Mg 4.5, Mn 0.7 (wt%) Optical microscope, interferential contrast 100 μm |
|
Micrograph
842
:
Macrograph of a resistance spot weld made in two plates of 1,5mm thickness. T3 - solution heat treatment, cold working and natural ageing. System: Al-Cu, Composition: Al, Cu 4.5, Mg 1.5 (wt%) Optical microscope, interferential contrast 1 mm |
|
Micrograph
843
:
Micrograph of base metal. T6 - solution heat treated and artificially aged. System: Al-Mg-Si, Composition: Al, Mg 1, Si 0.8, Mn 0.5 (wt%) Optical microscope, reflected light 250 μm |
|
Micrograph
844
:
Microstructure of extruded tube in Magnesium alloy AZ91 in direction perpendicular to the direction of extrusion. System: Mg-Al, Composition: Mg, Al 9.2, Zn 0.8 (wt %) Optical microscope, reflected light 500 μm |
|
Micrograph
845
:
Microstructure of extruded tube in Magnesium alloy AZ91 in direction perpendicular to the direction of extrusion. System: Mg-Al, Composition: Mg, Al 9.2, Zn 0.8 (wt %) Optical microscope, reflected light 50 μm |
Showing 51 - 60 of 60 micrographs | Page 1 2 3 4 5 6 | Previous | Next |
Help is available on browsing.
Alternatively, search the Library (from top right on any page), or use advanced search.