DoITPoMS Micrograph Library Browse the Library

Browse the Library

Categories > Metal or alloy > Keyword: nickel

34 micrographs available, ordered by micrograph number.


Showing 1 - 10 of 34 micrographs Page 1 2 3 4 | Previous | Next

Link to full record for micrograph 10 Micrograph 10 : Cu 70, Ni 30 (wt%), cored dendrites
System: Cu-Ni, Composition: Cu 70, Ni 30 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 11 Micrograph 11 : Cu 70, Ni 30 (wt%), cored dendrites
System: Cu-Ni, Composition: Cu 70, Ni 30 (wt%)
Reflected light microscopy
80 μm
Link to full record for micrograph 45 Micrograph 45 : Fe, Ni 30, C 0.3 (wt%), quenched - martensite plates
System: Fe-C-X, Composition: Fe, C 0.3, Ni 30 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 46 Micrograph 46 : Fe, Ni 30, C 0.3 (wt%), quenched - martensite plates
System: Fe-C-X, Composition: Fe, C 0.3, Ni 30 (wt%)
Reflected light microscopy
80 μm
Link to full record for micrograph 72 Micrograph 72 : Ni-hard iron
System: Fe-C-X, Composition: Fe, C 2.8, Ni 4.5, Mn 1.2, Cr 0.75, Si 0.5, P 0.3, Mo 0.25, S 0.1 (wt% typical) (Ni-hard iron)
Reflected light microscopy
400 μm
Link to full record for micrograph 73 Micrograph 73 : Ni-hard iron
System: Fe-C-X, Composition: Fe, C 2.8, Ni 4.5, Mn 1.2, Cr 0.75, Si 0.5, P 0.3, Mo 0.25, S 0.1 (wt% typical) (Ni-hard iron)
Reflected light microscopy
80 μm
Link to full record for micrograph 79 Micrograph 79 : Ni-superalloy, fatigue crack propagation
System: Ni-X, Composition: Not specified (Ni-Superalloy)
Scanning electron microscopy (SEM)
150 μm
Link to full record for micrograph 80 Micrograph 80 : Ni-superalloy, fatigue crack propagation
System: Ni-X, Composition: Not specified (Ni-Superalloy)
Scanning electron microscopy (SEM)
80 μm
Link to full record for micrograph 81 Micrograph 81 : Ni-superalloy, fatigue crack propagation
System: Ni-X, Composition: Not specified (Ni-Superalloy)
Scanning electron microscopy (SEM)
30 μm
Link to full record for micrograph 390 Micrograph 390 : Nickel hard cast iron, martensitic
System: Fe-C-X, Composition: Fe, C 2.95, Si 0.60, Mn 0.60, Ni 4.00, Cr 1.90 (wt%)
Reflected light microscopy
400 μm