Browse the Library
Categories > Metal or alloy > Keyword: silicon
32 micrographs available, ordered by micrograph number.
Showing 1 - 10 of 32 micrographs | Page 1 2 3 4 | Previous | Next |
Micrograph
58
:
Al 88, Si 12 (wt%), eutectic alloy System: Al-Si, Composition: Al 88, Si 12 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
59
:
Al 88, Si 12 (wt%), eutectic alloy System: Al-Si, Composition: Al 88, Si 12 (wt%) Reflected light microscopy 80 μm |
|
Micrograph
60
:
Al, Si 12, Na 0.02 (wt%), eutectic alloy - refined microstructure System: Al-Si-Na, Composition: Al, Si 12, Na 0.02 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
61
:
Al, Si 12, Na 0.02 (wt%), eutectic alloy - refined microstructure System: Al-Si-Na, Composition: Al, Si 12, Na 0.02 (wt%) Reflected light microscopy 80 μm |
|
Micrograph
62
:
Fe, C 3.6, Si 2.1 (wt%), hypereutectic grey cast iron System: Fe-C-X, Composition: Fe, C 3.6, Si 2.1 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
63
:
Fe, C 3.6, Si 2.1 (wt%), hypereutectic grey cast iron System: Fe-C-X, Composition: Fe, C 3.6, Si 2.1 (wt%) Reflected light microscopy 40 μm |
|
Micrograph
64
:
Fe, C 3.6, Si 2.1, Mg 0.07 (wt%), spheroidal graphite System: Fe-C-X, Composition: Fe, C 3.6, Si 2.1, Mg 0.07 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
65
:
Fe, C 3.6, Si 2.1, Mg 0.07 (wt%), spheroidal graphite System: Fe-C-X, Composition: Fe, C 3.6, Si 2.1, Mg 0.07 (wt%) Reflected light microscopy 80 μm |
|
Micrograph
70
:
Silal System: Fe-C-X, Composition: Fe, C 3.0, Si 6, Mn 0.7, P 0.3, S 0.1 (wt% typical) (Silal) Reflected light microscopy 200 μm |
|
Micrograph
71
:
Silal System: Fe-C-X, Composition: Fe, C 3.0, Si 6, Mn 0.7, P 0.3, S 0.1 (wt% typical) (Silal) Reflected light microscopy 80 μm |