Austempered ductile cast iron System: Fe-C-X, Composition: Fe, C 3.52, Si 2.51, Mn 0.49, Mo 0.15, Cu 0.31 (wt%) Reflected light microscopy 20 μm |
|
Micrograph
843
:
Micrograph of base metal. T6 - solution heat treated and artificially aged. System: Al-Mg-Si, Composition: Al, Mg 1, Si 0.8, Mn 0.5 (wt%) Optical microscope, reflected light 250 μm |