Browse the Library
Categories > Metal or alloy > Keyword: carbon
256 micrographs available, ordered by micrograph number.
Showing 91 - 100 of 256 micrographs | Page 1 .. 7 8 9 10 11 12 13 .. 26 | Previous | Next |
Micrograph
270
:
Fe, C 0.6 (wt%) steel, hard drawn System: Fe-C-X, Composition: Fe, C 0.6 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
271
:
Fe, C 0.07, Mn 2.3 (wt%) steel, carburised at 950°C System: Fe-C-X, Composition: Fe, C 0.07, Mn 2.2 (wt%) Reflected light microscopy 800 μm |
|
Micrograph
272
:
Fe, C 0.07, Mn 2.3 (wt%) steel, carburised at 950°C System: Fe-C-X, Composition: Fe, C 0.07, Mn 2.2 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
273
:
Fe, C 0.07, Mn 2.3 (wt%) steel, carburised at 950°C System: Fe-C-X, Composition: Fe, C 0.07, Mn 2.2 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
274
:
Fe, C 0.07, Mn 2.3 (wt%) steel, carburised at 950°C System: Fe-C-X, Composition: Fe, C 0.07, Mn 2.2 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
275
:
Fe, C 0.07, Mn 2.3 (wt%) steel, carburised at 950°C System: Fe-C-X, Composition: Fe, C 0.07, Mn 2.2 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
276
:
Fe, C 0.07, Mn 2.3 (wt%) steel, carburised at 950°C System: Fe-C-X, Composition: Fe, C 0.07, Mn 2.2 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
277
:
Fe, C 0.07, Mn 2.3 (wt%) steel, carburised at 950°C System: Fe-C-X, Composition: Fe, C 0.07, Mn 2.2 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
278
:
Fe, C 2, Mn 0.7 (wt%) steel, quenched, producing martensite System: Fe-C-X, Composition: Fe, C 0.55, Mn 0.65 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
279
:
Fe, C 2, Mn 0.7 (wt%) steel, quenched, producing martensite and cracking System: Fe-C-X, Composition: Fe, C 0.55, Mn 0.65 (wt%) Reflected light microscopy 200 μm |
Showing 91 - 100 of 256 micrographs | Page 1 .. 7 8 9 10 11 12 13 .. 26 | Previous | Next |
Help is available on browsing.
Alternatively, search the Library (from top right on any page), or use advanced search.