Browse the Library
Categories > Metal or alloy > Reflected light microscopy > Keyword: carbon
242 micrographs available, ordered by micrograph number.
Showing 191 - 200 of 242 micrographs | Page 1 .. 17 18 19 20 21 22 23 .. 25 | Previous | Next |
Micrograph
385
:
As cast white cast iron System: Fe-C-X, Composition: Fe, C 2.3, Mn 4.0 (wt%) Reflected light microscopy 100 μm |
|
Micrograph
386
:
As cast white cast iron System: Fe-C-X, Composition: Fe, C 2.3, Mn 4.0 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
387
:
Silal System: Fe-C-X, Composition: Fe, C 2.10, Si 5.60, Mn 0.50 (wt%) (Silal) Reflected light microscopy 400 μm |
|
Micrograph
388
:
Silal System: Fe-C-X, Composition: Fe, C 2.10, Si 5.60, Mn 0.50 (wt%) (Silal) Reflected light microscopy 200 μm |
|
Micrograph
389
:
Silal System: Fe-C-X, Composition: Fe, C 2.10, Si 5.60, Mn 0.50 (wt%) (Silal) Reflected light microscopy 100 μm |
|
Micrograph
393
:
Cast iron with magnesium induced spheroidised graphite System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 400 μm |
|
Micrograph
394
:
Cast iron with magnesium induced spheroidised graphite System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 200 μm |
|
Micrograph
395
:
Cast iron with magnesium induced spheroidised graphite System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 100 μm |
|
Micrograph
396
:
Cast iron with magnesium induced spheroidised graphite System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 400 μm |
|
Micrograph
398
:
Cast iron with magnesium induced spheroidised graphite System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 200 μm |
Showing 191 - 200 of 242 micrographs | Page 1 .. 17 18 19 20 21 22 23 .. 25 | Previous | Next |
Help is available on browsing.
Alternatively, search the Library (from top right on any page), or use advanced search.