Micrograph
387
:
Silal System: Fe-C-X, Composition: Fe, C 2.10, Si 5.60, Mn 0.50 (wt%) (Silal) Reflected light microscopy 400 μm |
|
Micrograph
388
:
Silal System: Fe-C-X, Composition: Fe, C 2.10, Si 5.60, Mn 0.50 (wt%) (Silal) Reflected light microscopy 200 μm |
|
Micrograph
389
:
Silal System: Fe-C-X, Composition: Fe, C 2.10, Si 5.60, Mn 0.50 (wt%) (Silal) Reflected light microscopy 100 μm |
|
Micrograph
393
:
Cast iron with magnesium induced spheroidised graphite System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 400 μm |
|
Micrograph
394
:
Cast iron with magnesium induced spheroidised graphite System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 200 μm |
|
Micrograph
395
:
Cast iron with magnesium induced spheroidised graphite System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 100 μm |
|
Micrograph
396
:
Cast iron with magnesium induced spheroidised graphite System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 400 μm |
|
Micrograph
397
:
Cast iron with magnesium induced spheroidised graphite System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy, polarised 400 μm |
|
Micrograph
398
:
Cast iron with magnesium induced spheroidised graphite System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 200 μm |
|
Micrograph
399
:
Cast iron with magnesium induced spheroidised graphite System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 100 μm |
Showing 201 - 210 of 256 micrographs | Page 1 .. 18 19 20 21 22 23 24 .. 26 | Previous | Next |
Help is available on browsing.
Alternatively, search the Library (from top right on any page), or use advanced search.