Micrograph
400
:
Cast iron with magnesium induced spheroidised graphite System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 400 μm |
|
Micrograph
401
:
Cast iron with magnesium induced spheroidised graphite System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 100 μm |
|
Micrograph
402
:
Cast iron with magnesium induced spheroidised graphite System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 100 μm |
|
Micrograph
403
:
Cast iron with magnesium induced spheroidised graphite System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 400 μm |
|
Micrograph
404
:
Cast iron with magnesium induced spheroidised graphite System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 200 μm |
|
Micrograph
405
:
Cast iron with magnesium induced spheroidised graphite System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 100 μm |
|
Micrograph
406
:
Cast iron, containing phosphorus System: Fe-C-X, Composition: Fe, C 3.46, Si 0.12, Mn 0.33, P 1.91, Cr 1.02 (wt%) Reflected light microscopy 800 μm |
|
Micrograph
407
:
Cast iron, containing phosphorus System: Fe-C-X, Composition: Fe, C 3.46, Si 0.12, Mn 0.33, P 1.91, Cr 1.02 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
408
:
Cast iron, containing phosphorus System: Fe-C-X, Composition: Fe, C 3.46, Si 0.12, Mn 0.33, P 1.91, Cr 1.02 (wt%) Reflected light microscopy 100 μm |
|
Micrograph
409
:
Cast iron, containing phosphorus System: Fe-C-X, Composition: Fe, C 3.46, Si 0.12, Mn 0.33, P 1.91, Cr 1.02 (wt%) Reflected light microscopy 800 μm |
Showing 211 - 220 of 256 micrographs | Page 1 .. 19 20 21 22 23 24 25 26 | Previous | Next |
Help is available on browsing.
Alternatively, search the Library (from top right on any page), or use advanced search.