Browse the Library
Categories > Metal or alloy > Keyword: cast iron
69 micrographs available, ordered by micrograph number.
| Showing 1 - 10 of 69 micrographs | Page 1 2 3 4 5 6 7 | Previous | Next |
![]() |
Micrograph
62
:
Fe, C 3.6, Si 2.1 (wt%), hypereutectic grey cast iron System: Fe-C-X, Composition: Fe, C 3.6, Si 2.1 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
63
:
Fe, C 3.6, Si 2.1 (wt%), hypereutectic grey cast iron System: Fe-C-X, Composition: Fe, C 3.6, Si 2.1 (wt%) Reflected light microscopy 40 μm |
![]() |
Micrograph
66
:
Hypoeutectic white cast iron System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 400 μm |
![]() |
Micrograph
67
:
Hypoeutectic white cast iron System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 80 μm |
![]() |
Micrograph
68
:
Grey cast iron core with white cast iron periphery System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 200 μm |
![]() |
Micrograph
69
:
Grey cast iron core with white cast iron periphery System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 40 μm |
![]() |
Micrograph
72
:
Ni-hard iron System: Fe-C-X, Composition: Fe, C 2.8, Ni 4.5, Mn 1.2, Cr 0.75, Si 0.5, P 0.3, Mo 0.25, S 0.1 (wt% typical) (Ni-hard iron) Reflected light microscopy 400 μm |
![]() |
Micrograph
73
:
Ni-hard iron System: Fe-C-X, Composition: Fe, C 2.8, Ni 4.5, Mn 1.2, Cr 0.75, Si 0.5, P 0.3, Mo 0.25, S 0.1 (wt% typical) (Ni-hard iron) Reflected light microscopy 80 μm |
![]() |
Micrograph
353
:
Pearlitic malleable cast iron System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 800 μm |
![]() |
Micrograph
354
:
Pearlitic malleable cast iron System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 400 μm |