Micrograph
222
:
Low carbon steel from bottom of wood screw. System: Fe-C-X, Composition: Fe, C very low (wt%) Reflected light microscopy 800 μm |
![]() |
Micrograph
223
:
Annealed low carbon steel with carbides System: Fe-C-X, Composition: Fe, C low (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
224
:
Annealed low carbon steel with carbides System: Fe-C-X, Composition: Fe, C low (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
225
:
Normalised steel System: Fe-C-X, Composition: Fe, C 0.55 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
226
:
Normalised steel System: Fe-C-X, Composition: Fe, C 0.55 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
227
:
Normalised steel System: Fe-C-X, Composition: Fe, C 0.4 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
228
:
Normalised steel System: Fe-C-X, Composition: Fe, C 0.4 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
229
:
Normalised steel System: Fe-C-X, Composition: Fe, C 0.5 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
230
:
Normalised steel System: Fe-C-X, Composition: Fe, C 0.5 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
231
:
Normalised steel System: Fe-C-X, Composition: Fe, C 0.6 (wt%) Reflected light microscopy 400 μm |
| Showing 121 - 130 of 708 micrographs | Page 1 .. 10 11 12 13 14 15 16 .. 71 | Previous | Next |
Help is available on browsing.
Alternatively, search the Library (from top right on any page), or use advanced search.