Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Browse the Library
Categories > Metal or alloy
708 micrographs available, ordered by micrograph number.
| Showing 131 - 140 of 708 micrographs | Page 1 .. 11 12 13 14 15 16 17 .. 71 | Previous | Next |
![]() |
Micrograph
232
:
Normalised steel System: Fe-C-X, Composition: Fe, C 0.6 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
233
:
Hypoeutectoid steel, normalised at 1100°C System: Fe-C-X, Composition: Fe, C 0.4 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
234
:
Hypoeutectoid steel, normalised at 1100°C System: Fe-C-X, Composition: Fe, C 0.4 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
235
:
Hypoeutectoid steel, normalised at 950°C System: Fe-C-X, Composition: Fe, C 0.4 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
236
:
Hypoeutectoid steel, normalised at 950°C System: Fe-C-X, Composition: Fe, C 0.4 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
237
:
Hypoeutectoid steel, normalised at 950°C System: Fe-C-X, Composition: Fe, C 0.4 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
238
:
Hypoeutectoid steel, normalised at 950°C System: Fe-C-X, Composition: Fe, C 0.4 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
239
:
Fe, C 0.4, Mn 0.8 (wt%) steel, normalised System: Fe-C-X, Composition: Fe, C 0.4, Mn 0.8 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
240
:
Fe, C 0.4, Mn 0.8 (wt%) steel, normalised System: Fe-C-X, Composition: Fe, C 0.4, Mn 0.8 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
241
:
Fe, C 0.3 (wt%) steel, spheroidised carbide System: Fe-C-X, Composition: Fe, C 0.3 (wt%) Reflected light microscopy 400 μm |
| Showing 131 - 140 of 708 micrographs | Page 1 .. 11 12 13 14 15 16 17 .. 71 | Previous | Next |