Link to full record for micrograph 372 Micrograph 372 : As cast white cast iron
System: Fe-C-X, Composition: Fe, C 3.62, Si 0.33, Mn 0.38, Cr 0.89 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 373 Micrograph 373 : As cast white cast iron
System: Fe-C-X, Composition: Fe, C 3.62, Si 0.33, Mn 0.38, Cr 0.89 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 374 Micrograph 374 : Fully transformed ledeburite cast iron
System: Fe-C-X, Composition: Fe, C 4.17, Si 0.40, Mn 0.45, Cr 0.95 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 375 Micrograph 375 : Fully transformed ledeburite cast iron
System: Fe-C-X, Composition: Fe, C 4.17, Si 0.40, Mn 0.45, Cr 0.95 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 376 Micrograph 376 : As cast white cast iron
System: Fe-C-X, Composition: Fe, C 3.56, Si 0.20, Mn 0.37, Cr 0.91 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 377 Micrograph 377 : As cast white cast iron
System: Fe-C-X, Composition: Fe, C 3.56, Si 0.20, Mn 0.37, Cr 0.91 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 378 Micrograph 378 : Grey cast iron with significant Si content
System: Fe-C-X, Composition: Fe, C 3.52, Si 3.26, Mn 0.47 (wt%) (Grey cast iron)
Reflected light microscopy
400 μm
Link to full record for micrograph 379 Micrograph 379 : Grey cast iron with significant Si content
System: Fe-C-X, Composition: Fe, C 3.52, Si 3.26, Mn 0.47 (wt%) (Grey cast iron)
Reflected light microscopy
200 μm
Link to full record for micrograph 380 Micrograph 380 : Grey cast iron with significant Si content
System: Fe-C-X, Composition: Fe, C 3.52, Si 3.26, Mn 0.47 (wt%) (Grey cast iron)
Reflected light microscopy
100 μm
Link to full record for micrograph 381 Micrograph 381 : Grey cast iron
System: Fe-C-X, Composition: Grey cast iron
Reflected light microscopy
400 μm

Showing 261 - 270 of 708 micrographs Page 1 .. 24 25 26 27 28 29 30 .. 71 | Previous | Next