Micrograph
790
:
Austempered ductile cast iron System: Fe-C-X, Composition: Fe, C 3.52, Si 2.51, Mn 0.49, Mo 0.15, Cu 0.31 (wt%) Reflected light microscopy 20 μm |
![]() |
Micrograph
791
:
Austempered ductile cast iron System: Fe-C-X, Composition: Fe, C 3.52, Si 2.51, Mn 0.49, Mo 0.15, Cu 0.31 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
792
:
Austempered ductile cast iron System: Fe-C-X, Composition: Fe, C 3.52, Si 2.51, Mn 0.49, Mo 0.15, Cu 0.31 (wt%) Reflected light microscopy 20 μm |
![]() |
Micrograph
793
:
Austempered ductile cast iron System: Fe-C-X, Composition: Fe, C 3.52, Si 2.51, Mn 0.49, Mo 0.15, Cu 0.31 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
794
:
Austempered ductile cast iron System: Fe-C-X, Composition: Fe, C 3.52, Si 2.51, Mn 0.49, Mo 0.15, Cu 0.31 (wt%) Reflected light microscopy 20 μm |
![]() |
Micrograph
795
:
Blackheart cast iron System: Fe-C-X, Composition: Blackheart cast iron Reflected light microscopy 100 μm |
![]() |
Micrograph
796
:
Blackheart cast iron System: Fe-C-X, Composition: Blackheart cast iron Reflected light microscopy 100 μm |
![]() |
Micrograph
797
:
Wear-resistant high-chromium cast iron System: Fe-C-X, Composition: Fe, C 2.6, Cr 17, Mo 2, Ni 2 (wt%) Reflected light microscopy 40 μm |
![]() |
Micrograph
798
:
Wear-resistant high-chromium cast iron System: Fe-C-X, Composition: Fe, C 2.6, Cr 17, Mo 2, Ni 2 (wt%) Reflected light microscopy 20 μm |
![]() |
Micrograph
799
:
Austenitic stainless steel solution treated, water quenched and tempered System: Fe-C-X, Composition: Stainless steel with Cr 18, Ni 10, Nb 1 (wt%) Scanning electron microscopy (SEM) 2 μm |
Showing 541 - 550 of 592 micrographs | Page 1 .. 52 53 54 55 56 57 58 .. 60 | Previous | Next |
Help is available on browsing.
Alternatively, search the Library (from top right on any page), or use advanced search.