Browse the Library
Categories > Metal or alloy > Cu-Sn
61 micrographs available, ordered by micrograph number.
| Showing 1 - 10 of 61 micrographs | Page 1 2 3 4 5 6 7 | Previous | Next |
![]() |
Micrograph
12
:
Cu 21, Sn 79 (wt%), peritectic transformation System: Cu-Sn, Composition: Cu 21, Sn 79 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
13
:
Cu 21, Sn 79 (wt%), peritectic transformation System: Cu-Sn, Composition: Cu 21, Sn 79 (wt%) Reflected light microscopy 80 μm |
![]() |
Micrograph
437
:
Cu, Sn 20 (wt%) bronze, exhibiting dendritic solidification System: Cu-Sn, Composition: Cu 80, Sn 20 (wt%) Reflected light microscopy 800 μm |
![]() |
Micrograph
438
:
Cu, Sn 20 (wt%) bronze, exhibiting dendritic solidification System: Cu-Sn, Composition: Cu 80, Sn 20 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
481
:
Cu 80, Sn 20 (wt%) bronze, as cast System: Cu-Sn, Composition: Cu 80, Sn 20 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
482
:
Cu 80, Sn 20 (wt%) bronze, as cast System: Cu-Sn, Composition: Cu 80, Sn 20 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
483
:
Cu 80, Sn 20 (wt%) bronze, as cast System: Cu-Sn, Composition: Cu 80, Sn 20 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
484
:
Cu 80, Sn 20 (wt%) bronze, exhibiting dendritic solidification System: Cu-Sn, Composition: Cu 85, Sn 15 (wt%) Reflected light microscopy 800 μm |
![]() |
Micrograph
485
:
Cu 80, Sn 20 (wt%) bronze, exhibiting dendritic solidification System: Cu-Sn, Composition: Cu 85, Sn 15 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
486
:
Cu 80, Sn 20 (wt%) bronze, exhibiting dendritic solidification System: Cu-Sn, Composition: Cu 85, Sn 15 (wt%) Reflected light microscopy 100 μm |
| Showing 1 - 10 of 61 micrographs | Page 1 2 3 4 5 6 7 | Previous | Next |