Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Browse the Library
Categories > Metal or alloy > Cu
3 micrographs available, ordered by micrograph number.
![]() |
Micrograph
142
:
Tough pitch copper, failed by fibrous ductile fracture. System: Cu, Composition: Tough pitch copper Scanning electron microscopy (SEM) 20 μm |
![]() |
Micrograph
435
:
Tough pitch' nearly pure copper, with oxygen impurity System: Cu, Composition: Cu 99.7 (wt%), some oxygen Reflected light microscopy 400 μm |
![]() |
Micrograph
436
:
Tough pitch' nearly pure copper, with oxygen impurity System: Cu, Composition: Cu 99.7 (wt%), some oxygen Reflected light microscopy 200 μm |
Help is available on browsing.