Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Browse the Library
Categories > Metal or alloy > Al-Sn
1 micrograph available, ordered by micrograph number.
![]() |
Micrograph
613
:
Facetted aluminium dendrites System: Al-Sn, Composition: Al 15, Sn 85 (wt%) Reflected light microscopy 80 μm |
Help is available on browsing.