Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Browse the Library
Categories > Metal or alloy > Ni-X
21 micrographs available, ordered by micrograph number.
| Showing 1 - 10 of 21 micrographs | Page 1 2 3 | Previous | Next |
![]() |
Micrograph
79
:
Ni-superalloy, fatigue crack propagation System: Ni-X, Composition: Not specified (Ni-Superalloy) Scanning electron microscopy (SEM) 150 μm |
![]() |
Micrograph
80
:
Ni-superalloy, fatigue crack propagation System: Ni-X, Composition: Not specified (Ni-Superalloy) Scanning electron microscopy (SEM) 80 μm |
![]() |
Micrograph
81
:
Ni-superalloy, fatigue crack propagation System: Ni-X, Composition: Not specified (Ni-Superalloy) Scanning electron microscopy (SEM) 30 μm |
![]() |
Micrograph
713
:
IN718 nickel-based superalloy held for 1 minute at 850°C System: Ni-X, Composition: Ni 53, Fe 19, Cr 18, Nb 5 (wt% approx) + small amounts of Ti, Mo, Co, Al Reflected light microscopy, cross-polarised, with Nomarski filter 20 μm |
![]() |
Micrograph
714
:
IN718 nickel-based superalloy held for 20 minutes at 850°C System: Ni-X, Composition: Ni 53, Fe 19, Cr 18, Nb 5 (wt% approx) + small amounts of Ti, Mo, Co, Al Reflected light microscopy, cross-polarised, with Nomarski filter 20 μm |
![]() |
Micrograph
715
:
IN718 nickel-based superalloy held for 1 hour at 850°C System: Ni-X, Composition: Ni 53, Fe 19, Cr 18, Nb 5 (wt% approx) + small amounts of Ti, Mo, Co, Al Reflected light microscopy, cross-polarised, with Nomarski filter 25 μm |
![]() |
Micrograph
716
:
IN718 nickel-based superalloy held for 3 hours at 850°C System: Ni-X, Composition: Ni 53, Fe 19, Cr 18, Nb 5 (wt% approx) + small amounts of Ti, Mo, Co, Al Reflected light microscopy, cross-polarised, with Nomarski filter 25 μm |
![]() |
Micrograph
717
:
IN718 nickel-based superalloy held for 6 hours at 850°C System: Ni-X, Composition: Ni 53, Fe 19, Cr 18, Nb 5 (wt% approx) + small amounts of Ti, Mo, Co, Al Reflected light microscopy, cross-polarised, with Nomarski filter 25 μm |
![]() |
Micrograph
718
:
IN718 nickel-based superalloy held for 24 hours at 850°C System: Ni-X, Composition: Ni 53, Fe 19, Cr 18, Nb 5 (wt% approx) + small amounts of Ti, Mo, Co, Al Reflected light microscopy, cross-polarised, with Nomarski filter 25 μm |
![]() |
Micrograph
719
:
IN718 nickel-based superalloy held for 48 hours at 850°C System: Ni-X, Composition: Ni 53, Fe 19, Cr 18, Nb 5 (wt% approx) + small amounts of Ti, Mo, Co, Al Reflected light microscopy, cross-polarised, with Nomarski filter 25 μm |
| Showing 1 - 10 of 21 micrographs | Page 1 2 3 | Previous | Next |
Help is available on browsing.
Alternatively, search the Library (from top right on any page), or use advanced search.