Categories > Metal or alloy > Mg-Al > Mg, Al 9.2, Zn 0.8 (wt %) > Keyword: magnesium

2 micrographs available, ordered by micrograph number.


Link to full record for micrograph 844 Micrograph 844 : Microstructure of extruded tube in Magnesium alloy AZ91 in direction perpendicular to the direction of extrusion.
System: Mg-Al, Composition: Mg, Al 9.2, Zn 0.8 (wt %)
Optical microscope, reflected light
500 μm
Link to full record for micrograph 845 Micrograph 845 : Microstructure of extruded tube in Magnesium alloy AZ91 in direction perpendicular to the direction of extrusion.
System: Mg-Al, Composition: Mg, Al 9.2, Zn 0.8 (wt %)
Optical microscope, reflected light
50 μm