Categories > Metal or alloy > Cu-Zn > Cu 80, Zn 20 (wt%) > Reflected light microscopy
6 micrographs available, ordered by micrograph number.
Micrograph
431
:
Cu 80, Zn 20 (wt%), recrystallised - annealing twins System: Cu-Zn, Composition: Cu 80, Zn 20 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
432
:
Cu 80, Zn 20 (wt%), recrystallised - annealing twins System: Cu-Zn, Composition: Cu 80, Zn 20 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
477
:
Cu 80, Zn 20 (wt%) brass, exhibiting dendritic solidification System: Cu-Zn, Composition: Cu 80, Zn 20 (wt%) Reflected light microscopy 800 μm |
|
Micrograph
478
:
Cu 80, Zn 20 (wt%) brass, exhibiting dendritic solidification System: Cu-Zn, Composition: Cu 80, Zn 20 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
479
:
Cu 80, Zn 20 (wt%) brass, exhibiting dendritic solidification System: Cu-Zn, Composition: Cu 80, Zn 20 (wt%) Reflected light microscopy 100 μm |
|
Micrograph
480
:
Cu 80, Zn 20 (wt%) brass, exhibiting dendritic solidification System: Cu-Zn, Composition: Cu 80, Zn 20 (wt%) Reflected light microscopy 100 μm |