Categories > Metal or alloy > Cu-Zn > Reflected light microscopy > Keyword: copper
63 micrographs available, ordered by micrograph number.
Showing 51 - 60 of 63 micrographs | Page 1 2 3 4 5 6 7 | Previous | Next |
Micrograph
468
:
Cu 50, Zn 50 (wt%) brass, as cast System: Cu-Zn, Composition: Cu 50, Zn 50 (wt%) Reflected light microscopy 800 μm |
|
Micrograph
469
:
Cu 50, Zn 50 (wt%) brass, as cast System: Cu-Zn, Composition: Cu 50, Zn 50 (wt%) Reflected light microscopy 800 μm |
|
Micrograph
470
:
Cu 50, Zn 50 (wt%) brass, as cast System: Cu-Zn, Composition: Cu 50, Zn 50 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
471
:
Cu 50, Zn 50 (wt%) brass, as cast System: Cu-Zn, Composition: Cu 50, Zn 50 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
472
:
Cu 50, Zn 50 (wt%) brass, chill cast System: Cu-Zn, Composition: Cu 50, Zn 50 (wt%) Reflected light microscopy 800 μm |
|
Micrograph
473
:
Cu 50, Zn 50 (wt%) brass, chill cast System: Cu-Zn, Composition: Cu 50, Zn 50 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
474
:
Cu 50, Zn 50 (wt%) brass, chill cast System: Cu-Zn, Composition: Cu 50, Zn 50 (wt%) Reflected light microscopy 100 μm |
|
Micrograph
475
:
Cu 55, Zn 45 (wt%) brass, cast annealed System: Cu-Zn, Composition: Cu 52, Zn 45 (wt%) Reflected light microscopy 800 μm |
|
Micrograph
476
:
Cu 55, Zn 45 (wt%) brass, cast annealed System: Cu-Zn, Composition: Cu 52, Zn 45 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
477
:
Cu 80, Zn 20 (wt%) brass, exhibiting dendritic solidification System: Cu-Zn, Composition: Cu 80, Zn 20 (wt%) Reflected light microscopy 800 μm |