Categories > Metal or alloy > Fe-C-X > Fe, C 2.85, Si 0.33, Mn 0.39, Cr 0.91 (wt%) > Keyword: white cast iron

2 micrographs available, ordered by micrograph number.


Link to full record for micrograph 370 Micrograph 370 : As cast white cast iron
System: Fe-C-X, Composition: Fe, C 2.85, Si 0.33, Mn 0.39, Cr 0.91 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 371 Micrograph 371 : As cast white cast iron
System: Fe-C-X, Composition: Fe, C 2.85, Si 0.33, Mn 0.39, Cr 0.91 (wt%)
Reflected light microscopy
100 μm