Categories > Metal or alloy > Fe-C-X > Stainless steel > Keyword: recrystallisation

5 micrographs available, ordered by micrograph number.


Link to full record for micrograph 772 Micrograph 772 : Austenitic stainless steel
System: Fe-C-X, Composition: Stainless steel
Transmission electron microscopy (TEM)
1 μm
Link to full record for micrograph 773 Micrograph 773 : Austenitic stainless steel
System: Fe-C-X, Composition: Stainless steel
Transmission electron microscopy (TEM)
1 μm
Link to full record for micrograph 774 Micrograph 774 : Austenitic stainless steel
System: Fe-C-X, Composition: Stainless steel
Transmission electron microscopy (TEM)
1 μm
Link to full record for micrograph 775 Micrograph 775 : Austenitic stainless steel
System: Fe-C-X, Composition: Stainless steel
Transmission electron microscopy (TEM)
1 μm
Link to full record for micrograph 776 Micrograph 776 : Austenitic stainless steel
System: Fe-C-X, Composition: Stainless steel
Transmission electron microscopy (TEM)
2 μm