Categories > Metal or alloy > Fe-C-X > Stainless steel with Cr 15, Ni 35, Ti 5, C 0.1 > Keyword: austenite

1 micrograph available, ordered by micrograph number.


Link to full record for micrograph 817 Micrograph 817 : Austenitic stainless steel tempered
System: Fe-C-X, Composition: Stainless steel with Cr 15, Ni 35, Ti 5, C 0.1
Scanning electron microscopy (SEM)
2 μm