Categories > Metal or alloy > Fe-C-X > Fe, C 0.07, Mn 2.2 (wt%) > Reflected light microscopy

7 micrographs available, ordered by micrograph number.


Link to full record for micrograph 271 Micrograph 271 : Fe, C 0.07, Mn 2.3 (wt%) steel, carburised at 950°C
System: Fe-C-X, Composition: Fe, C 0.07, Mn 2.2 (wt%)
Reflected light microscopy
800 μm
Link to full record for micrograph 272 Micrograph 272 : Fe, C 0.07, Mn 2.3 (wt%) steel, carburised at 950°C
System: Fe-C-X, Composition: Fe, C 0.07, Mn 2.2 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 273 Micrograph 273 : Fe, C 0.07, Mn 2.3 (wt%) steel, carburised at 950°C
System: Fe-C-X, Composition: Fe, C 0.07, Mn 2.2 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 274 Micrograph 274 : Fe, C 0.07, Mn 2.3 (wt%) steel, carburised at 950°C
System: Fe-C-X, Composition: Fe, C 0.07, Mn 2.2 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 275 Micrograph 275 : Fe, C 0.07, Mn 2.3 (wt%) steel, carburised at 950°C
System: Fe-C-X, Composition: Fe, C 0.07, Mn 2.2 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 276 Micrograph 276 : Fe, C 0.07, Mn 2.3 (wt%) steel, carburised at 950°C
System: Fe-C-X, Composition: Fe, C 0.07, Mn 2.2 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 277 Micrograph 277 : Fe, C 0.07, Mn 2.3 (wt%) steel, carburised at 950°C
System: Fe-C-X, Composition: Fe, C 0.07, Mn 2.2 (wt%)
Reflected light microscopy
200 μm