Browse the Library
Categories > Metal or alloy > Fe-C-X > Reflected light microscopy > Keyword: white cast iron
17 micrographs available, ordered by micrograph number.
Showing 1 - 10 of 17 micrographs | Page 1 2 | Previous | Next |
Micrograph
362
:
White cast iron, subject to slow heating and cooling treatment System: Fe-C-X, Composition: Fe, C 3.4, Si 0.35, Mn 0.22 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
363
:
White cast iron, subject to slow heating and cooling treatment System: Fe-C-X, Composition: Fe, C 3.4, Si 0.35, Mn 0.22 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
364
:
White cast iron, subject to slow heating and cooling treatment System: Fe-C-X, Composition: Fe, C 3.4, Si 0.35, Mn 0.22 (wt%) Reflected light microscopy 100 μm |
|
Micrograph
365
:
As cast white cast iron System: Fe-C-X, Composition: Fe, C 3.4, Si 0.35, Mn 0.22 (wt%), + ... Reflected light microscopy 200 μm |
|
Micrograph
366
:
Whiteheart cast iron System: Fe-C-X, Composition: Fe, C 3.4, Si 0.35, Mn 0.22 (wt%), + ... Reflected light microscopy 400 μm |
|
Micrograph
367
:
Whiteheart cast iron System: Fe-C-X, Composition: Fe, C 3.4, Si 0.35, Mn 0.22 (wt%), + ... Reflected light microscopy 200 μm |
|
Micrograph
368
:
Blackheart cast iron System: Fe-C-X, Composition: Fe, C 2.4, Si 1.1, Mn 1.1 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
369
:
Blackheart cast iron System: Fe-C-X, Composition: Fe, C 2.4, Si 1.1, Mn 1.1 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
370
:
As cast white cast iron System: Fe-C-X, Composition: Fe, C 2.85, Si 0.33, Mn 0.39, Cr 0.91 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
371
:
As cast white cast iron System: Fe-C-X, Composition: Fe, C 2.85, Si 0.33, Mn 0.39, Cr 0.91 (wt%) Reflected light microscopy 100 μm |
Showing 1 - 10 of 17 micrographs | Page 1 2 | Previous | Next |
Help is available on browsing.
Alternatively, search the Library (from top right on any page), or use advanced search.