Browse the Library
Categories > Metal or alloy > Fe-C-X > Reflected light microscopy > Keyword: nickel
9 micrographs available, ordered by micrograph number.
Micrograph
45
:
Fe, Ni 30, C 0.3 (wt%), quenched - martensite plates System: Fe-C-X, Composition: Fe, C 0.3, Ni 30 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
46
:
Fe, Ni 30, C 0.3 (wt%), quenched - martensite plates System: Fe-C-X, Composition: Fe, C 0.3, Ni 30 (wt%) Reflected light microscopy 80 μm |
|
Micrograph
72
:
Ni-hard iron System: Fe-C-X, Composition: Fe, C 2.8, Ni 4.5, Mn 1.2, Cr 0.75, Si 0.5, P 0.3, Mo 0.25, S 0.1 (wt% typical) (Ni-hard iron) Reflected light microscopy 400 μm |
|
Micrograph
73
:
Ni-hard iron System: Fe-C-X, Composition: Fe, C 2.8, Ni 4.5, Mn 1.2, Cr 0.75, Si 0.5, P 0.3, Mo 0.25, S 0.1 (wt% typical) (Ni-hard iron) Reflected light microscopy 80 μm |
|
Micrograph
390
:
Nickel hard cast iron, martensitic System: Fe-C-X, Composition: Fe, C 2.95, Si 0.60, Mn 0.60, Ni 4.00, Cr 1.90 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
391
:
Nickel hard cast iron, martensitic System: Fe-C-X, Composition: Fe, C 2.95, Si 0.60, Mn 0.60, Ni 4.00, Cr 1.90 (wt%) Reflected light microscopy 100 μm |
|
Micrograph
392
:
Nickel hard cast iron, martensitic System: Fe-C-X, Composition: Fe, C 2.95, Si 0.60, Mn 0.60, Ni 4.00, Cr 1.90 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
797
:
Wear-resistant high-chromium cast iron System: Fe-C-X, Composition: Fe, C 2.6, Cr 17, Mo 2, Ni 2 (wt%) Reflected light microscopy 40 μm |
|
Micrograph
798
:
Wear-resistant high-chromium cast iron System: Fe-C-X, Composition: Fe, C 2.6, Cr 17, Mo 2, Ni 2 (wt%) Reflected light microscopy 20 μm |
Help is available on browsing.