Browse the Library
Categories > Metal or alloy > Fe-C-X > Reflected light microscopy
268 micrographs available, ordered by micrograph number.
Showing 51 - 60 of 268 micrographs | Page 1 .. 3 4 5 6 7 8 9 .. 27 | Previous | Next |
Micrograph
225
:
Normalised steel System: Fe-C-X, Composition: Fe, C 0.55 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
226
:
Normalised steel System: Fe-C-X, Composition: Fe, C 0.55 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
227
:
Normalised steel System: Fe-C-X, Composition: Fe, C 0.4 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
228
:
Normalised steel System: Fe-C-X, Composition: Fe, C 0.4 (wt%) Reflected light microscopy 100 μm |
|
Micrograph
229
:
Normalised steel System: Fe-C-X, Composition: Fe, C 0.5 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
230
:
Normalised steel System: Fe-C-X, Composition: Fe, C 0.5 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
231
:
Normalised steel System: Fe-C-X, Composition: Fe, C 0.6 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
232
:
Normalised steel System: Fe-C-X, Composition: Fe, C 0.6 (wt%) Reflected light microscopy 100 μm |
|
Micrograph
233
:
Hypoeutectoid steel, normalised at 1100°C System: Fe-C-X, Composition: Fe, C 0.4 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
234
:
Hypoeutectoid steel, normalised at 1100°C System: Fe-C-X, Composition: Fe, C 0.4 (wt%) Reflected light microscopy 200 μm |
Showing 51 - 60 of 268 micrographs | Page 1 .. 3 4 5 6 7 8 9 .. 27 | Previous | Next |
Help is available on browsing.
Alternatively, search the Library (from top right on any page), or use advanced search.