Browse the Library
Categories > Metal or alloy > Cu-Sn > Cu 80, Sn 20 (wt%) > Reflected light microscopy
8 keywords available. The number of micrographs available is given in [brackets].
- alloy [13]
- Show relevant: micrographs
- annealing [8]
- Show relevant: micrographs
- bronze [13]
- Show relevant: micrographs
- copper [13]
- Show relevant: micrographs
- dendrite [5]
- Show relevant: micrographs
- metal [13]
- Show relevant: micrographs
- tin [10]
- Show relevant: micrographs
- zinc [3]
- Show relevant: micrographs
Help is available on browsing.