Categories > Metal or alloy > Cu-Sn > Cu 95, Sn 5, P 0.15 (wt% approx.) > Keyword: alloy

4 micrographs available, ordered by micrograph number.


Link to full record for micrograph 500 Micrograph 500 : Cu - 5% Sn phosphor bronze
System: Cu-Sn, Composition: Cu 95, Sn 5, P 0.15 (wt% approx.)
Reflected light microscopy
800 μm
Link to full record for micrograph 501 Micrograph 501 : Cu - 5% Sn phosphor bronze
System: Cu-Sn, Composition: Cu 95, Sn 5, P 0.15 (wt% approx.)
Reflected light microscopy
400 μm
Link to full record for micrograph 502 Micrograph 502 : Cu - 5% Sn phosphor bronze
System: Cu-Sn, Composition: Cu 95, Sn 5, P 0.15 (wt% approx.)
Reflected light microscopy
200 μm
Link to full record for micrograph 503 Micrograph 503 : Cu - 5% Sn phosphor bronze
System: Cu-Sn, Composition: Cu 95, Sn 5, P 0.15 (wt% approx.)
Reflected light microscopy
100 μm