Categories > Metal or alloy > Cu-Sn > Cu 21, Sn 79 (wt%) > Keyword: bronze

2 micrographs available, ordered by micrograph number.


Link to full record for micrograph 12 Micrograph 12 : Cu 21, Sn 79 (wt%), peritectic transformation
System: Cu-Sn, Composition: Cu 21, Sn 79 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 13 Micrograph 13 : Cu 21, Sn 79 (wt%), peritectic transformation
System: Cu-Sn, Composition: Cu 21, Sn 79 (wt%)
Reflected light microscopy
80 μm