Categories > Metal or alloy > Al-Cu > Al 75, Cu 25 (wt%) > Keyword: aluminium
2 micrographs available, ordered by micrograph number.
Micrograph
1
:
Al 75, Cu 25 (wt%), hypoeutectic alloy System: Al-Cu, Composition: Al 75, Cu 25 (wt%) Reflected light microscopy 40 μm |
|
Micrograph
2
:
Al 75, Cu 25 (wt%), hypoeutectic alloy System: Al-Cu, Composition: Al 75, Cu 25 (wt%) Scanning electron microscopy (SEM) 30 μm |