Categories > Metal or alloy > Cu > Cu 99.7 (wt%), some oxygen > Reflected light microscopy
2 micrographs available, ordered by micrograph number.
Micrograph
435
:
Tough pitch' nearly pure copper, with oxygen impurity System: Cu, Composition: Cu 99.7 (wt%), some oxygen Reflected light microscopy 400 μm |
|
Micrograph
436
:
Tough pitch' nearly pure copper, with oxygen impurity System: Cu, Composition: Cu 99.7 (wt%), some oxygen Reflected light microscopy 200 μm |