Categories > Metal or alloy > Al-Mg > Al 90, Mg 10 (wt%) > Transmission electron microscopy (TEM)
1 micrograph available, ordered by micrograph number.
Micrograph
614
:
Rapid solidification in an atomised droplet System: Al-Mg, Composition: Al 90, Mg 10 (wt%) Transmission electron microscopy (TEM) 500 nm |