Categories > Metal or alloy > Reflected light microscopy > Keyword: quenching
64 micrographs available, ordered by micrograph number.
Showing 21 - 30 of 64 micrographs | Page 1 2 3 4 5 6 7 | Previous | Next |
Micrograph
300
:
Fe, C 0.75 (wt%) steel, quenched, martensitic and manganese sulphides System: Fe-C-X, Composition: Fe, C 0.75 (wt%) Reflected light microscopy 100 μm |
|
Micrograph
301
:
Fe, C 0.55 (wt%) steel, quenched and tempered System: Fe-C-X, Composition: Fe, C 0.55 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
302
:
Fe, C 0.55 (wt%) steel, quenched and tempered System: Fe-C-X, Composition: Fe, C 0.55 (wt%) Reflected light microscopy 100 μm |
|
Micrograph
303
:
Fe, C 0.3 (wt%) steel, quenched and tempered System: Fe-C-X, Composition: Fe, C 0.3 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
304
:
Fe, C 0.3 (wt%) steel, quenched and tempered System: Fe-C-X, Composition: Fe, C 0.3 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
305
:
Fe, C 0.3 (wt%) steel, quenched and tempered System: Fe-C-X, Composition: Fe, C 0.3 (wt%) Reflected light microscopy 100 μm |
|
Micrograph
309
:
Fe, C 0.4 (wt%) steel, slow quenched System: Fe-C-X, Composition: Fe, C 0.4 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
310
:
Fe, C 0.4 (wt%) steel, slow quenched System: Fe-C-X, Composition: Fe, C 0.4 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
311
:
Fe, C 0.4 (wt%) steel, slow quenched System: Fe-C-X, Composition: Fe, C 0.4 (wt%) Reflected light microscopy 100 μm |
|
Micrograph
312
:
Fe, C 0.4 (wt%) steel, slow quenched System: Fe-C-X, Composition: Fe, C 0.4 (wt%) Reflected light microscopy 100 μm |