Categories > Metal or alloy > Reflected light microscopy > Keyword: twinning
12 micrographs available, ordered by micrograph number.
Showing 11 - 12 of 12 micrographs | Page 1 2 | Previous | Next |
Micrograph
43
:
Fe, C 0.2 (wt%), explosively deformed - mechanical twins System: Fe-C-X, Composition: Fe, C 0.2 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
44
:
Fe, C 0.2 (wt%), explosively deformed - mechanical twins System: Fe-C-X, Composition: Fe, C 0.2 (wt%) Reflected light microscopy 80 μm |