Browse the Library
Categories > Metal or alloy > Reflected light microscopy
509 micrographs available, ordered by micrograph number.
Showing 501 - 509 of 509 micrographs | Page 1 .. 45 46 47 48 49 50 51 | Previous | Next |
Micrograph
954
:
Afunfun, Niger. Melilith-pyroxene-copper slag System: Cu production, Composition: Not specified Reflected light microscopy 200 μm |
|
Micrograph
955
:
Afunfun, Niger. Melilith-pyroxene-copper slag System: Cu production, Composition: Not specified Reflected light microscopy 100 μm |
|
Micrograph
956
:
Carthage, smithing slag, phoenician System: Smithing slag, Composition: Not specified Reflected light microscopy 500 μm |
|
Micrograph
957
:
Kupferberg, Fichtel mountain, Germany. Speiss from copper production System: Cu production, Composition: Not specified Reflected light microscopy 200 μm |
|
Micrograph
958
:
Kupferberg, Fichtel mountain, Germany. Speiss from copper production System: Cu production, Composition: Not specified Reflected light microscopy 100 μm |
|
Micrograph
961
:
Torud, Central Iran. Copper slag System: Cu production, Composition: Not specified Reflected light microscopy 500 μm |
|
Micrograph
964
:
Torud, Central Iran. Copper slag System: Cu production, Composition: Not specified Reflected light microscopy 500 μm |
|
Micrograph
966
:
Morro-de-Mezquitilla, Malaga, Spain. Iron smithing slag System: Pre-Roman Ag production, Composition: Not specified Reflected light microscopy 200 μm |
|
Micrograph
970
:
Elisenhof, Juetland, Germany. Medieval smithing slag System: Smithing slag, Composition: Not specified Reflected light microscopy 200 μm |
Showing 501 - 509 of 509 micrographs | Page 1 .. 45 46 47 48 49 50 51 | Previous | Next |