Browse the Library
Categories > Metal or alloy > Scanning electron microscopy (SEM)
48 micrographs available, ordered by micrograph number.
Showing 41 - 48 of 48 micrographs | Page 1 2 3 4 5 | Previous | Next |
Micrograph
818
:
Austenitic stainless steel tempered System: Fe-C-X, Composition: Stainless steel with Cr 15, Ni 35, Nb 2.5, C 0.1 (wt%) Scanning electron microscopy (SEM) 4 μm |
|
Micrograph
820
:
Austenitic stainless steel tempered System: Fe-C-X, Composition: Stainless steel with Cr 15, Ni 35, Nb 5, C O.1 (wt%) Scanning electron microscopy (SEM) 4 μm |
|
Micrograph
821
:
Austenitic stainless steel impact deformed at room temperature System: Fe-C-X, Composition: Fe, C 1.15, Mn 13 (wt%) Scanning electron microscopy (SEM) 2.5 μm |
|
Micrograph
826
:
Austenitic stainless steel tempered, with Mo2 and M6C precipitates System: Fe-C-X, Composition: Fe, C 0.20, Mo 3.8, Ta 0.22 (wt%) Scanning electron microscopy (SEM) 2.5 μm |
|
Micrograph
831
:
Austenitic stainless steel water quenched, with a-martensite needles within lamellae System: Fe-C-X, Composition: Fe, C 0.12, Mn 14.2, Cr 13.7 Scanning electron microscopy (SEM) 4 μm |
|
Micrograph
834
:
Steel slowly cooled, fracture surface of commercial ingot System: Fe-C-X, Composition: Fe, C 0.13, Ni 4, Cr 2, Mn 0.49, S 0.015 (wt%) Scanning electron microscopy (SEM) 4 μm |
|
Micrograph
855
:
Low Carbon Steel System: Fe-C-X, Composition: Fe, C low (wt%) Scanning electron microscopy (SEM) 20 μm |
|
Micrograph
856
:
Low Carbon Steel System: Fe-C-X, Composition: Fe, C low (wt%) Scanning electron microscopy (SEM) 5 μm |
Showing 41 - 48 of 48 micrographs | Page 1 2 3 4 5 | Previous | Next |
Help is available on browsing.
Alternatively, search the Library (from top right on any page), or use advanced search.