Browse the Library
Categories > Metal or alloy > Reflected light microscopy, polarised > Keyword: alloy
3 micrographs available, ordered by micrograph number.
Micrograph
397
:
Cast iron with magnesium induced spheroidised graphite System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy, polarised 400 μm |
|
Micrograph
604
:
Extruded aluminium System: Al, Composition: Commercial purity (99.5%) Reflected light microscopy, polarised 40 μm |
|
Micrograph
609
:
The grain structure of extruded aluminium System: Al, Composition: Commercial purity (99.5%) Reflected light microscopy, polarised 40 μm |
Help is available on browsing.