Categories > Polymer composite > Araldite (TM) > Cross-polarised light microscopy > Keyword: load distribution

3 micrographs available, ordered by micrograph number.


Link to full record for micrograph 597 Micrograph 597 : Frozen stress photoelastic fringe pattern during fibre pushout
System: Araldite (TM), Composition: Araldite CT200/HT907 'matrix' with cylindrical CT200/HT901 'fibre'
Cross-polarised light microscopy
6 mm
Link to full record for micrograph 598 Micrograph 598 : Frozen stress photoelastic assessment of load distribution around a cylinder
System: Araldite (TM), Composition: Araldite CT200/HT907 'matrix' with cylindrical CT200/HT901 'fibre'
Cross-polarised light microscopy
6 mm
Link to full record for micrograph 599 Micrograph 599 : Frozen stress photoelastic assessment of load distribution around an ellipsoid
System: Araldite (TM), Composition: Araldite CT200/HT907 'matrix' with ellipsoid CT200/HT901 'particle'
Cross-polarised light microscopy
6 mm