Dissemination of IT for the Promotion of Materials Science (DoITPoMS)

DoITPoMS Micrograph Library Browse the Library

Browse the Library

Categories > Polymer composite > Araldite (TM) > Cross-polarised light microscopy > Keyword: pushout

1 micrograph available, ordered by micrograph number.


Link to full record for micrograph 597 Micrograph 597 : Frozen stress photoelastic fringe pattern during fibre pushout
System: Araldite (TM), Composition: Araldite CT200/HT907 'matrix' with cylindrical CT200/HT901 'fibre'
Cross-polarised light microscopy
6 mm

Help is available on browsing.

Alternatively, search the Library (from top right on any page), or use advanced search.