Categories > Fracture > Forging steel
1 micrograph available, ordered by micrograph number.
![]() |
Micrograph
78
:
Forging steel, brittle, intergranular fracture System: Fe-C-X, Composition: Forging steel Scanning electron microscopy (SEM) 800 μm |