Link to full record for micrograph 139 Micrograph 139 : Al-Mg-Si, failed through microvoid coalescence.
System: Al-Mg-Si, Composition: Al, Si 1.2, Mg 0.4 (wt%) (AA6016)
Scanning electron microscopy (SEM)
40 μm
Link to full record for micrograph 140 Micrograph 140 : Al-Mg-Si, failed through microvoid coalescence.
System: Al-Mg-Si, Composition: Al, Si 1.2, Mg 0.4 (wt%) (AA6016)
Scanning electron microscopy (SEM)
40 μm
Link to full record for micrograph 141 Micrograph 141 : Al-Mg-Si, failed through microvoid coalescence.
System: Al-Mg-Si, Composition: Al, Si 1.2, Mg 0.4 (wt%) (AA6016)
Scanning electron microscopy (SEM)
40 μm
Link to full record for micrograph 142 Micrograph 142 : Tough pitch copper, failed by fibrous ductile fracture.
System: Cu, Composition: Tough pitch copper
Scanning electron microscopy (SEM)
20 μm
Link to full record for micrograph 143 Micrograph 143 : Notched low carbon ferritic steel, failed through cleavage.
System: Fe-C-X, Composition: Not specified
Scanning electron microscopy (SEM)
20 μm
Link to full record for micrograph 144 Micrograph 144 : Zinc, notched specimen, failed through brittle cleavage fracture.
System: Zn, Composition: Not specified
Scanning electron microscopy (SEM)
200 μm
Link to full record for micrograph 145 Micrograph 145 : Zinc, notched specimen, failed through brittle cleavage fracture.
System: Zn, Composition: Not specified
Scanning electron microscopy (SEM)
1 mm
Link to full record for micrograph 146 Micrograph 146 : HY100 forging steel, notched impact specimen, failed through brittle intergranular fracture.
System: Fe-C-X, Composition: Not specified
Scanning electron microscopy (SEM)
200 μm
Link to full record for micrograph 147 Micrograph 147 : HY100 forging steel, notched impact specimen, failed through brittle intergranular fracture.
System: Fe-C-X, Composition: Not specified
Scanning electron microscopy (SEM)
200 μm
Link to full record for micrograph 560 Micrograph 560 : Crazing near a fracture surface in polystyrene
System: Polystyrene (PS), Composition: Not specified
Photography (no microscope)
10 mm