Categories > Fracture > Polystyrene (PS) > Not specified > Photography (no microscope) > Keyword: fracture
1 micrograph available, ordered by micrograph number.
Micrograph
560
:
Crazing near a fracture surface in polystyrene System: Polystyrene (PS), Composition: Not specified Photography (no microscope) 10 mm |