Link to full record for micrograph 650 Micrograph 650 : Small ceramic pot showing centimetre scale crystals within the glaze
System: Soda-lime-silica glaze, Composition: Soda-lime-silica glaze containing zinc oxide 25, cobalt oxide 0.5 (wt%)
Photography (no microscope)
20 mm
Link to full record for micrograph 655 Micrograph 655 : Small ceramic pot showing centimetre scale crystals within the glaze
System: Soda-lime-silica glaze, Composition: Soda-lime-silica glaze containing zinc oxide 25, cobalt oxide 0.5 (wt%)
Photography (no microscope)
5 mm