Categories > Ceramic > ZrO2 84, Yb2O3 16 (wt%)
1 micrograph available, ordered by micrograph number.
![]() |
Micrograph
847
:
Plasma sprayed (PS) partially stabilised zirconia (PSZ) showing splat morphology System: ZrO2-Yb2O3, Composition: ZrO2 84, Yb2O3 16 (wt%) Field emission gun scanning electron microscopy (FEGSEM) 2 μm |