Categories > Ceramic > ZrO2 92.5, Y2O3 7.5 (wt%) > Field emission gun scanning electron microscopy (FEGSEM) > Keyword: partially stabilized zirconia (PSZ)
1 micrograph available, ordered by micrograph number.
Micrograph
848
:
Physical vapour deposited (PVD) partially stabilized zirconia (PSZ) showing columnar structure System: ZrO2-Y2O3, Composition: ZrO2 92.5, Y2O3 7.5 (wt%) Field emission gun scanning electron microscopy (FEGSEM) 1 μm |