Categories > Ceramic > BaO . 6Fe2O3 > Reflected light microscopy > Keyword: oxygen

1 micrograph available, ordered by micrograph number.


Link to full record for micrograph 152 Micrograph 152 : Barium Hexaferrite
System: BaO-Fe2O3, Composition: BaO . 6Fe2O3
Reflected light microscopy
100 μm