Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Browse the Library
Categories > Ceramic > Not specified (LAS: Li2O-Al2O3-SiO2)
6 micrographs available, ordered by micrograph number.
![]() |
Micrograph
160
:
Glass ceramic, heat treated at 750° C for 3 hours System: LAS: Li2O-Al2O3-SiO2, Composition: Not specified Transmitted polarised light microscopy, with sensitive tint plate 100 μm |
![]() |
Micrograph
161
:
Glass ceramic, heat treated at 750°C for 3 hours System: LAS: Li2O-Al2O3-SiO2, Composition: Not specified Transmitted polarised light microscopy 100 μm |
![]() |
Micrograph
162
:
Glass ceramic, heat treated at 840°C for 3 hours System: LAS: Li2O-Al2O3-SiO2, Composition: Not specified Transmitted polarised light microscopy, with sensitive tint plate 100 μm |
![]() |
Micrograph
163
:
Glass ceramic, heat treated at 840°C for 3 hours System: LAS: Li2O-Al2O3-SiO2, Composition: Not specified Transmitted polarised light microscopy 100 μm |
![]() |
Micrograph
164
:
Glass ceramic, heat treated at 900°C for 3 hours System: LAS: Li2O-Al2O3-SiO2, Composition: Not specified Transmitted polarised light microscopy, with sensitive tint plate 100 μm |
![]() |
Micrograph
165
:
Glass ceramic, heat treated at 900°C for 3 hours System: LAS: Li2O-Al2O3-SiO2, Composition: Not specified Transmitted polarised light microscopy 100 μm |
Help is available on browsing.
Alternatively, search the Library (from top right on any page), or use advanced search.