Link to full record for micrograph 185 Micrograph 185 : Silicon Nitride-bonded Silicon Carbide
System: Silicon nitride-bonded silicon carbide, Composition: Particles of SiC in a reaction-bonded Si3N4 matrix
Reflected light microscopy
250 μm
Link to full record for micrograph 186 Micrograph 186 : Silicon Carbide from within a Silicon Nitride-bonded Silicon Carbide sample
System: Silicon nitride-bonded silicon carbide, Composition: Particles of SiC in a reaction-bonded Si3N4 matrix
Reflected light microscopy
25 μm